top of page
Pulsed HVOF –
Thermo Spray Detonation Gun
-
Particles velocity speed – Ultrasound (over 1200 m/s)
-
Coating porosity – 0.5%
-
Deposited Materials
– Metals and alloys
– Ceramics – Al2O3
– Composites – WC/Co
– Combinations of above
Please see the table below for a list of sample processes.
-
WC-based coatings with hardness of up to 1300 HV300
-
Al2O3-based coatings with hardness of up to 1300 HV300
-
Ti-based coatings with hardness of up to 1000 HV300
-
Coating porosity typically below 0.5%
-
Low compressive residual stresses in coatings
-
Negligible oxide content in coatings